The material is from local place of the terra-cotta musuem.very precious and nice.we put the clay in the room to leaven about 2 weeks.then begain to work.
A man step on the clay to make it more sticky.
The different parts of warriors is made by individual mold.
Smooth the outline,Carve the detail and make the face different.
Check the detail and mend it.
Keep firing about 2 weeks.
Put the air-dried warriors in the kiln,build up the door to fire.
After 5 days baked ,the warriors were moved out from the kilns .then they will be finished .
Uncolored warriors will be put outside to check their quality .Keeped in the rain and sunshine about 1 .5 month .If they are no cracks ,they are in good condition .